Aluminium · Aluminium, conductor and sheet grade · isotropic
EN AW-1050A O/H111
EN 485-2 · soft (O/H111) sheet
EN AW-1050A O/H111 is an aluminium grade for conductors and sheet to EN 485-2. Its minimum 0.2 % proof strength is 20 MPa. E = 69 GPa and α = 23.5 × 10⁻⁶/K (typical values).
- Record
- al-1050a-o
- Library
- v1.1.0
- Properties
- 7
- Sources
- 1
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
isotropic| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| E | Young's modulus | 69 | GPa | typical | [1] |
Physical, thermal and electrical
at 20 °C| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| α | Coefficient of thermal expansion ⓘ 20–100 °C | 23.5 | 10⁻⁶/K | typical | [1] |
| ρ | Density | 2700 | kg/m³ | typical | [1] |
| λ | Thermal conductivity ⓘ lower end of the datasheet range | 210 (210 – 220) | W/(m·K) | typical | [1] |
| σ_e | Electrical conductivity ⓘ lower end of the datasheet range | 34 (34 – 36) | MS/m | typical | [1] |
Strength
a band applies up to and including its upper limitSources
every value names onemin product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). EN AW-1050A O/H111 — material properties, EN 485-2. Library v1.1.0, record al-1050a-o. https://staging.badgermecx.com/materials/al-1050a-o/ (accessed 2026-11-26).
@misc{badgermecx_al1050ao,
title = {EN AW-1050A O/H111 -- material properties, EN 485-2},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record al-1050a-o},
url = {https://staging.badgermecx.com/materials/al-1050a-o/}
}