Composite · UD lamina, carbon · orthotropic
T300/5208 carbon/epoxy
Kaw, Table 2.1 · V_f = 0.70
T300/5208 carbon/epoxy is a unidirectional carbon-fibre lamina to Kaw, Table 2.1. Its typical longitudinal tensile strength is 1500 MPa. Along the fibres E₁ = 181 GPa; across them E₂ = 10.3 GPa.
- Record
- ud-t300-5208
- Library
- v1.1.0
- Properties
- 13
- Sources
- 1
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
orthotropicPhysical, thermal and electrical
at 20 °CStrength
a band applies up to and including its upper limit| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| X_t | Longitudinal tensile strength | 1500 | MPa | typical | [1] |
| X_c | Longitudinal compressive strength | 1500 | MPa | typical | [1] |
| Y_t | Transverse tensile strength | 40 | MPa | typical | [1] |
| Y_c | Transverse compressive strength | 246 | MPa | typical | [1] |
| S₁₂ | In-plane shear strength | 68 | MPa | typical | [1] |
Notes
- Plane-stress (lamina) data: E₃, ν₁₃, ν₂₃, G₁₃ and G₂₃ are not given, so a 3D stiffness matrix is not formed. For a transversely isotropic lamina E₃ = E₂, G₁₃ = G₁₂ and ν₁₃ = ν₁₂; G₂₃ or ν₂₃ must come from elsewhere.
Sources
every value names one- A. K. Kaw, Mechanics of Composite Materials, 2nd ed., Table 2.1 (as reproduced in course material)Copies checked: 1, 2, 3, 4
min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). T300/5208 carbon/epoxy — material properties, Kaw, Table 2.1. Library v1.1.0, record ud-t300-5208. https://staging.badgermecx.com/materials/ud-t300-5208/ (accessed 2026-11-26).
@misc{badgermecx_udt3005208,
title = {T300/5208 carbon/epoxy -- material properties, Kaw, Table 2.1},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record ud-t300-5208},
url = {https://staging.badgermecx.com/materials/ud-t300-5208/}
}