Aluminium · Aluminium extrusions · isotropic
EN AW-6082 T5
EN 1999-1-1 · extrusions and drawn tube · buckling class B
EN AW-6082 T5 is an aluminium alloy and temper for extrusions to EN 1999-1-1. Its characteristic 0.2 % proof strength is 230–230 MPa, depending on the product form and thickness. E = 70 GPa, ν = 0.3 and α = 23 × 10⁻⁶/K (design values).
- Record
- al-6082-t5-ext
- Library
- v1.1.0
- Properties
- 11
- Sources
- 2
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
isotropic| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| E | Young's modulus ⓘ EN 1999-1-1 3.2.5 | 70 | GPa | design | [1] |
| G | Shear modulus | 27 | GPa | design | [1] |
| ν | Poisson's ratio | 0.3 | – | design | [1] |
| K | Bulk modulus K = E / 3(1 − 2ν) | 58.33 | GPa | derived | — |
| λ_L | Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) | 40.38 | GPa | derived | — |
| c₀ | Bar wave speed c₀ = √(E/ρ) | 5092 | m/s | derived | — |
Physical, thermal and electrical
at 20 °C| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| α | Coefficient of thermal expansion ⓘ for T < 100 °C | 23 | 10⁻⁶/K | design | [1] |
| ρ | Density | 2700 | kg/m³ | design | [1] |
| λ | Thermal conductivity ⓘ lower end of the datasheet range, 20 °C | 170 (170 – 220) | W/(m·K) | typical | [2] |
| σ_e | Electrical conductivity ⓘ lower end of the datasheet range, 20 °C | 24 (24 – 32) | MS/m | typical | [2] |
Strength
a band applies up to and including its upper limit| Property | Product form | Thickness | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|---|
| f_o | EP/O, EP/H — EP/O, EP/H | t ≤ 5 mm | 230 | MPa | char | [1] |
| f_u | EP/O, EP/H — EP/O, EP/H | t ≤ 5 mm | 270 | MPa | char | [1] |
| Symbol | Property | Value at t = 5 mm · EP/O, EP/H | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| f_o | 0.2 % proof strength ⓘ thickness is the upper limit of each row | 230 | MPa | char | [1] |
| f_u | Tensile strength (R_m) | 270 | MPa | char | [1] |
| f_o,haz | 0.2 % proof strength in the heat-affected zone ⓘ MIG welding; EN 1999-1-1 reduces HAZ values for TIG and thicker parts | 125 | MPa | char | [1] |
| f_u,haz | Tensile strength in the heat-affected zone | 185 | MPa | char | [1] |
Sources
every value names one- EN 1999-1-1:2007, Eurocode 9 — Design of aluminium structures, Table 3.2b and 3.2.5Copies checked: 1, 2, 3, 4
- Wieland aluminium datasheets: EN AW-1050A, 5083, 6061, 6082Copies checked: 1, 2, 3, 4
min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). EN AW-6082 T5 — material properties, EN 1999-1-1. Library v1.1.0, record al-6082-t5-ext. https://staging.badgermecx.com/materials/al-6082-t5-ext/ (accessed 2026-11-26).
@misc{badgermecx_al6082t5ext,
title = {EN AW-6082 T5 -- material properties, EN 1999-1-1},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record al-6082-t5-ext},
url = {https://staging.badgermecx.com/materials/al-6082-t5-ext/}
}