CuZn37 brass (CW508L) is a brass to EN 1652. E = 105 GPa, ν = 0.34 and α = 20.2 × 10⁻⁶/K (typical values).
- Record
- cuzn37
- Library
- v1.1.0
- Properties
- 8
- Sources
- 1
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
isotropicPhysical, thermal and electrical
at 20 °C| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| ρ | Density | 8440 | kg/m³ | typical | [1] |
| α | Coefficient of thermal expansion ⓘ 0–300 °C | 20.2 | 10⁻⁶/K | typical | [1] |
| λ | Thermal conductivity | 120 | W/(m·K) | typical | [1] |
| c_p | Specific heat capacity | 377 | J/(kg·K) | typical | [1] |
| σ_e | Electrical conductivity | 15 | MS/m | typical | [1] |
| IACS | Conductivity relative to annealed copper | 26 | % | typical | [1] |
| a | Thermal diffusivity a = λ / (ρ·c_p) | 37.71 | mm²/s | derived | — |
Notes
- Strength depends on the temper; see the producer's table.
Sources
every value names one- Wieland M37 (CuZn37, CW508L) datasheetCopies checked: 1
min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). CuZn37 brass (CW508L) — material properties, EN 1652. Library v1.1.0, record cuzn37. https://staging.badgermecx.com/materials/cuzn37/ (accessed 2026-11-26).
@misc{badgermecx_cuzn37,
title = {CuZn37 brass (CW508L) -- material properties, EN 1652},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record cuzn37},
url = {https://staging.badgermecx.com/materials/cuzn37/}
}