Timber · Solid timber, softwood · orthotropic

C16

EN 338:2016 · strength class, 12 % moisture reference

C16 is a softwood strength class to EN 338:2016. Its characteristic bending strength is 16 MPa. Along the fibres E₁ = 8 GPa; across them E₂ = 0.27 GPa.

Record
timber-c16
Library
v1.1.0
Properties
14
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E₁ · Modulus, direction 1 8GPa mean[1]
f_m,k · Bending strength 16MPa char[1]
f_t,0,k · Tension parallel to grain 8.5MPa char[1]
ρ · Density 370kg/m³ mean[1]

Elastic constants

orthotropic
SymbolPropertyValueUnitBasisRef.
E₁ Modulus, direction 1 ⓘ E_0,mean, along the grain 8 GPa mean [1]
E₀,₀₅ Modulus parallel to grain, 5 % fractile 5.4 GPa char [1]
E₂ Modulus, direction 2 ⓘ E_90,mean, across the grain 0.27 GPa mean [1]
E₃ Modulus, direction 3 ⓘ E_90,mean — the standard does not separate radial and tangential 0.27 GPa mean [1]
G₁₂ Shear modulus 1-2 ⓘ G_mean 0.5 GPa mean [1]
G₁₃ Shear modulus 1-3 ⓘ G_mean 0.5 GPa mean [1]

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density 370 kg/m³ mean [1]
ρ_k Density, characteristic (5 % fractile) 310 kg/m³ char [1]

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_m,k Bending strength 16 MPa char [1]
f_t,0,k Tension parallel to grain 8.5 MPa char [1]
f_t,90,k Tension perpendicular to grain 0.4 MPa char [1]
f_c,0,k Compression parallel to grain 17 MPa char [1]
f_c,90,k Compression perpendicular to grain 2.2 MPa char [1]
f_v,k Shear strength 3.2 MPa char [1]

Notes

  • EN 338 and EN 14080 give no Poisson's ratios; a 3D analysis needs them from another source.

Sources

every value names one
  1. EN 338:2016, Structural timber — Strength classes, Tables 1 and 3Copies checked: 1, 2, 3

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). C16 — material properties, EN 338:2016. Library v1.1.0, record timber-c16. https://staging.badgermecx.com/materials/timber-c16/ (accessed 2026-11-26).

@misc{badgermecx_timberc16,
  title  = {C16 -- material properties, EN 338:2016},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record timber-c16},
  url    = {https://staging.badgermecx.com/materials/timber-c16/}
}