Steel · Reinforcing steel · isotropic
B500B
EN 1992-1-1 Annex C · ductility class B
B500B is a reinforcing steel to EN 1992-1-1 Annex C. Its characteristic yield strength is 500 MPa. E = 200 GPa (design values).
- Record
- rebar-b500b
- Library
- v1.1.0
- Properties
- 5
- Sources
- 1
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
isotropic| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| E | Young's modulus ⓘ EN 1992-1-1 3.2.7(4) | 200 | GPa | design | [1] |
Physical, thermal and electrical
at 20 °C| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| ρ | Density ⓘ EN 1992-1-1 3.2.7(3) | 7850 | kg/m³ | mean | [1] |
Strength
a band applies up to and including its upper limitNotes
- Poisson's ratio and thermal expansion are not given by EN 1992-1-1 for reinforcement.
Sources
every value names one- EN 1992-1-1:2004, Eurocode 2 — Design of concrete structures, Table 3.1, 3.1.3, 3.2.7 and Annex CCopies checked: 1, 2, 3
min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). B500B — material properties, EN 1992-1-1 Annex C. Library v1.1.0, record rebar-b500b. https://staging.badgermecx.com/materials/rebar-b500b/ (accessed 2026-11-26).
@misc{badgermecx_rebarb500b,
title = {B500B -- material properties, EN 1992-1-1 Annex C},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record rebar-b500b},
url = {https://staging.badgermecx.com/materials/rebar-b500b/}
}