Copper · Copper · isotropic

Cu-ETP (CW004A, C11000)

EN 1652 / EN 13599 · R220, soft

Cu-ETP (CW004A, C11000) is a copper to EN 1652 / EN 13599. Its minimum yield strength is 140 MPa. E = 110 GPa and α = 16.8 × 10⁻⁶/K (typical values).

Record
cu-etp
Library
v1.1.0
Properties
8
Sources
2
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 110GPa typical[1]
f_y · Yield strength (R_eH / R_p0.2) 140MPa min[2]
f_u · Tensile strength (R_m) 220MPa min[2]
ρ · Density 8930kg/m³ typical[1]
α · Coefficient of thermal expansion 16.810⁻⁶/K typical[1]
λ · Thermal conductivity 394W/(m·K) typical[1]
c_p · Specific heat capacity 386J/(kg·K) typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus ⓘ annealed; 130 GPa cold-formed 110 (110 – 130) GPa typical [1]

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density ⓘ KME gives 8900 8930 kg/m³ typical [1]
α Coefficient of thermal expansion ⓘ 20–100 °C 16.8 10⁻⁶/K typical [1]
λ Thermal conductivity ⓘ at 20 °C; KME gives 385 394 (385 – 394) W/(m·K) typical [1]
c_p Specific heat capacity ⓘ at 20 °C 386 J/(kg·K) typical [1]
σ_e Electrical conductivity ⓘ DKI 57 MS/m, KME 58 MS/m (100 % IACS) 57 (57 – 58) MS/m typical [1,2]
a Thermal diffusivity a = λ / (ρ·c_p) 114.3 mm²/s derived —

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_u Tensile strength (R_m) ⓘ temper R220 (annealed): R_m 220–260 MPa 220 (220 – 260) MPa min [2]
f_y Yield strength (R_eH / R_p0.2) ⓘ temper R220: R_p0.2 given for information 140 MPa min [2]

Sources

every value names one
  1. Deutsches Kupferinstitut, Cu-ETP material datasheet (2005)Copies checked: 1
  2. KME / Kemper, Cu-ETP and Cu-OF rolled products datasheetsCopies checked: 1, 2

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). Cu-ETP (CW004A, C11000) — material properties, EN 1652 / EN 13599. Library v1.1.0, record cu-etp. https://staging.badgermecx.com/materials/cu-etp/ (accessed 2026-11-26).

@misc{badgermecx_cuetp,
  title  = {Cu-ETP (CW004A, C11000) -- material properties, EN 1652 / EN 13599},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record cu-etp},
  url    = {https://staging.badgermecx.com/materials/cu-etp/}
}

Export and related

SI units, every value with basis and source