Steel · Reinforcing steel · isotropic

B500A

EN 1992-1-1 Annex C · ductility class A

B500A is a reinforcing steel to EN 1992-1-1 Annex C. Its characteristic yield strength is 500 MPa. E = 200 GPa (design values).

Record
rebar-b500a
Library
v1.1.0
Properties
5
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 200GPa design[1]
f_y · Yield strength (R_eH / R_p0.2) 500MPa char[1]
ρ · Density 7850kg/m³ mean[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus ⓘ EN 1992-1-1 3.2.7(4) 200 GPa design [1]

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density ⓘ EN 1992-1-1 3.2.7(3) 7850 kg/m³ mean [1]

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_y Yield strength (R_eH / R_p0.2) ⓘ grade B500: f_yk = 500 MPa, within the 400–600 MPa range of Annex C 500 MPa char [1]
k Ratio (f_t/f_y)_k ⓘ k ≥ 1.05 1.05 – min [1]
ε_uk Strain at maximum force, characteristic 2.5 % min [1]

Notes

  • Poisson's ratio and thermal expansion are not given by EN 1992-1-1 for reinforcement.

Sources

every value names one
  1. EN 1992-1-1:2004, Eurocode 2 — Design of concrete structures, Table 3.1, 3.1.3, 3.2.7 and Annex CCopies checked: 1, 2, 3

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). B500A — material properties, EN 1992-1-1 Annex C. Library v1.1.0, record rebar-b500a. https://staging.badgermecx.com/materials/rebar-b500a/ (accessed 2026-11-26).

@misc{badgermecx_rebarb500a,
  title  = {B500A -- material properties, EN 1992-1-1 Annex C},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record rebar-b500a},
  url    = {https://staging.badgermecx.com/materials/rebar-b500a/}
}

Export and related

SI units, every value with basis and source