Nickel · Nickel alloy · isotropic
Alloy 625 (UNS N06625)
Special Metals INCONEL 625 · annealed, about 21 °C
Alloy 625 (UNS N06625) is a nickel alloy to Special Metals INCONEL 625. Its typical yield strength is 414 MPa. E = 207.5 GPa, ν = 0.278 (typical values).
- Record
- ni-625
- Library
- v1.1.0
- Properties
- 9
- Sources
- 1
- Build check
- passed ✓
- Viewing as
- guest
Elastic constants
isotropic| Symbol | Property | Value | Unit | Basis | Ref. |
|---|---|---|---|---|---|
| E | Young's modulus | 207.5 | GPa | typical | [1] |
| G | Shear modulus | 81.4 | GPa | typical | [1] |
| ν | Poisson's ratio | 0.278 | – | typical | [1] |
| K | Bulk modulus K = E / 3(1 − 2ν) | 155.8 | GPa | derived | — |
| λ_L | Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) | 101.7 | GPa | derived | — |
| c₀ | Bar wave speed c₀ = √(E/ρ) | 4958 | m/s | derived | — |
Physical, thermal and electrical
at 20 °CStrength
a band applies up to and including its upper limitSources
every value names one- Special Metals, INCONEL alloy 625 technical bulletinCopies checked: 1
min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown
Cite this page
for reports and papersBadgerMecX Materials (2026). Alloy 625 (UNS N06625) — material properties, Special Metals INCONEL 625. Library v1.1.0, record ni-625. https://staging.badgermecx.com/materials/ni-625/ (accessed 2026-11-26).
@misc{badgermecx_ni625,
title = {Alloy 625 (UNS N06625) -- material properties, Special Metals INCONEL 625},
author = {{BadgerMecX Materials}},
year = {2026},
note = {Library v1.1.0, record ni-625},
url = {https://staging.badgermecx.com/materials/ni-625/}
}